Rusty Red
by Brushing on SteelRusty Red imparts a Red Rust Finish upon Brushing or Dipping.
Steel Parts should be thoroughly cleaned and prepped prior to usage.
Directions:
- Prepare the Steel Surface by brushing SURCLEAN-400 to degrease and descale.
- Rinse with Water. Ensure no cleaning solution remains on surface.
- Brush Rusty Red on Surface until Surface is entirely covered. Pay attention to edges and hard to reach areas. Immediately upon brushing/dipping, a pink red finish will develop.
- Let Part sit for 1 hour to for the pink finish to become a Red Rust Finish. For better results, let the part sit for 12 hours.
- When part is completely dry and the rusting is complete, Seal the surface with an appropriate Lacquer for Metal.
Recommended Ancillary Products:
- SURCLEAN-400 Metal Conditioner
- Acrylaq-1045 FLAT Lacquer for Metal
Square Footage : Approximlately 90-100 Square Feet Per Gallon